File Download
Patent History
- ApplicationCN 20071305932 2004-04-19
- PublicationCN 101333611 2008-12-31
Patent Family
- CN 1806060 (A) 2006-07-19
- CN 100432257 (C) 2008-11-12
- CN 101333611 (A) 2008-12-31
- EP 1629133 (A1) 2006-03-01
- JP 2006523770 (A) 2006-10-19
- US 2004265614 (A1) 2004-12-30
- US 7306683 (B2) 2007-12-11
- US 2004230193 (A1) 2004-11-18
- US 7695471 (B2) 2010-04-13
- US 2008053575 (A1) 2008-03-06
- US 7789975 (B2) 2010-09-07
- WO 2004092431 (A1) 2004-10-28
Supplementary
-
Citations:
- Appears in Collections:
published patent: Shape memory material and method of making the same
Title | Shape memory material and method of making the same |
---|---|
Priority Date | 2003-04-18 US 10/464083P |
Inventors | |
Issue Date | 2008 |
Citation | China Published Patent Application CN 101333611. Beijing, PRC: State Intellectual Property Office (SIPO) of the P.R.C., 2008 How to Cite? |
Abstract | The present invention relates generally to a shape memory and/or super-elastic material, such as a nickel titanium alloy. Additionally or alternatively, the present invention relates to a super-elastic or pseudo-elastic material that has an initial transition temperature Af above a body temperature. The shape memory material can have a super-elasticity or pseudo-elasticity property at a temperature below the initial transition temperature Af of the material. For example, the shape memory material can have its workable temperature for producing super-elasticity or pseudo-elasticity of about 0 DEG C. to 15 DEG C. below the initial transition temperature Af. The shape memory material can be malleable at a room temperature, and become super-elastic or pseudo-elastic at a body temperature.; In addition, the present invention relates to a method of making a shape memory or a super-elastic material. The treatment protocols can include but not limited to thermo-mechanical, thermo-mechanical, radiation, and ternary alloying treatments. |
Persistent Identifier | http://hdl.handle.net/10722/176614 |
DC Field | Value | Language |
---|---|---|
dc.date.accessioned | 2012-11-30T08:38:14Z | - |
dc.date.available | 2012-11-30T08:38:14Z | - |
dc.date.issued | 2008 | - |
dc.identifier.citation | China Published Patent Application CN 101333611. Beijing, PRC: State Intellectual Property Office (SIPO) of the P.R.C., 2008 | en_HK |
dc.identifier.uri | http://hdl.handle.net/10722/176614 | - |
dc.description.abstract | The present invention relates generally to a shape memory and/or super-elastic material, such as a nickel titanium alloy. Additionally or alternatively, the present invention relates to a super-elastic or pseudo-elastic material that has an initial transition temperature Af above a body temperature. The shape memory material can have a super-elasticity or pseudo-elasticity property at a temperature below the initial transition temperature Af of the material. For example, the shape memory material can have its workable temperature for producing super-elasticity or pseudo-elasticity of about 0 DEG C. to 15 DEG C. below the initial transition temperature Af. The shape memory material can be malleable at a room temperature, and become super-elastic or pseudo-elastic at a body temperature.; In addition, the present invention relates to a method of making a shape memory or a super-elastic material. The treatment protocols can include but not limited to thermo-mechanical, thermo-mechanical, radiation, and ternary alloying treatments. | en_HK |
dc.title | Shape memory material and method of making the same | en_HK |
dc.type | Patent | en_US |
dc.description.nature | published_or_final_version | - |
dc.contributor.inventor | Chung, CY | en_HK |
dc.contributor.inventor | Cheung, KMC | - |
dc.contributor.inventor | Yeung, KWK | - |
dc.contributor.inventor | Lu, WW | - |
patents.identifier.application | CN 20071305932 | en_HK |
patents.identifier.application | ZL200710305932.7 | - |
patents.description.assignee | VERSITECH LTD [HK] | en_HK |
patents.description.country | China, PRC | en_HK |
patents.date.publication | 2008-12-31 | en_HK |
patents.identifier.hkutechid | O&T-2003-00105-3 | - |
patents.date.application | 2004-04-19 | en_HK |
patents.date.priority | 2003-04-18 US 10/464083P | en_HK |
patents.description.cc | CN | en_HK |
patents.identifier.publication | CN 101333611 | en_HK |
patents.relation.family | CN 1806060 (A) 2006-07-19 | en_HK |
patents.relation.family | CN 100432257 (C) 2008-11-12 | en_HK |
patents.relation.family | CN 101333611 (A) 2008-12-31 | en_HK |
patents.relation.family | EP 1629133 (A1) 2006-03-01 | en_HK |
patents.relation.family | JP 2006523770 (A) 2006-10-19 | en_HK |
patents.relation.family | US 2004265614 (A1) 2004-12-30 | en_HK |
patents.relation.family | US 7306683 (B2) 2007-12-11 | en_HK |
patents.relation.family | US 2004230193 (A1) 2004-11-18 | en_HK |
patents.relation.family | US 7695471 (B2) 2010-04-13 | en_HK |
patents.relation.family | US 2008053575 (A1) 2008-03-06 | en_HK |
patents.relation.family | US 7789975 (B2) 2010-09-07 | en_HK |
patents.relation.family | WO 2004092431 (A1) 2004-10-28 | en_HK |
patents.description.kind | A | en_HK |
patents.type | Patent_published | en_HK |