Article: Temperature and dimensional changes in the two-stage processing technique for complete dentures
Title | Temperature and dimensional changes in the two-stage processing technique for complete dentures |
---|---|
Authors | |
Keywords | Complete dentures Dimensional changes Temperature |
Issue Date | 1995 |
Publisher | Elsevier Ltd. The Journal's web site is located at http://www.elsevier.com/locate/jdent |
Citation | Journal Of Dentistry, 1995, v. 23 n. 4, p. 245-253 How to Cite? |
Abstract | Objectives: This study concerned the temperature and linear dimensional change of heat-cured acrylic resin in the two-stage processing technique for complete dentures. Methods: Thermocouples were incorporated in the acrylic resin for recording temperatures. Measurements between reference marks were made by a high-resolution digital measuring microscope. Results: No increase in temperature associated with the exothermic nature of the polymerization reaction was recorded. The temperature of the resin followed the waterbath temperature closely. The temperatures recorded at various regions were in phase with each other. The total linear shrinkage of the base after two processing cycles was less than 1% and compares favourably with studies on the single-stage processing technique. Conclusions: Temperature differential is excluded as a reason for the warpage of dentures. The dimensional changes of the denture base resulting from the two-stage processing technique cannot be considered to be of any clinical significance. © 1995. |
Persistent Identifier | http://hdl.handle.net/10722/66254 |
ISSN | 2023 Impact Factor: 4.8 2023 SCImago Journal Rankings: 1.313 |
ISI Accession Number ID |
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Yeung, KC | en_HK |
dc.contributor.author | Chow, TW | en_HK |
dc.contributor.author | Clark, RKF | en_HK |
dc.date.accessioned | 2010-09-06T05:44:50Z | - |
dc.date.available | 2010-09-06T05:44:50Z | - |
dc.date.issued | 1995 | en_HK |
dc.identifier.citation | Journal Of Dentistry, 1995, v. 23 n. 4, p. 245-253 | en_HK |
dc.identifier.issn | 0300-5712 | en_HK |
dc.identifier.uri | http://hdl.handle.net/10722/66254 | - |
dc.description.abstract | Objectives: This study concerned the temperature and linear dimensional change of heat-cured acrylic resin in the two-stage processing technique for complete dentures. Methods: Thermocouples were incorporated in the acrylic resin for recording temperatures. Measurements between reference marks were made by a high-resolution digital measuring microscope. Results: No increase in temperature associated with the exothermic nature of the polymerization reaction was recorded. The temperature of the resin followed the waterbath temperature closely. The temperatures recorded at various regions were in phase with each other. The total linear shrinkage of the base after two processing cycles was less than 1% and compares favourably with studies on the single-stage processing technique. Conclusions: Temperature differential is excluded as a reason for the warpage of dentures. The dimensional changes of the denture base resulting from the two-stage processing technique cannot be considered to be of any clinical significance. © 1995. | en_HK |
dc.language | eng | en_HK |
dc.publisher | Elsevier Ltd. The Journal's web site is located at http://www.elsevier.com/locate/jdent | en_HK |
dc.relation.ispartof | Journal of Dentistry | en_HK |
dc.rights | Journal of Dentistry. Copyright © Elsevier Ltd. | en_HK |
dc.subject | Complete dentures | - |
dc.subject | Dimensional changes | - |
dc.subject | Temperature | - |
dc.subject.mesh | Acrylic Resins - chemistry | en_HK |
dc.subject.mesh | Cold Temperature | en_HK |
dc.subject.mesh | Dental Casting Technique | en_HK |
dc.subject.mesh | Dental Impression Technique | en_HK |
dc.subject.mesh | Denture Bases | en_HK |
dc.subject.mesh | Denture, Complete | en_HK |
dc.subject.mesh | Hot Temperature | en_HK |
dc.subject.mesh | Polymers - chemistry | en_HK |
dc.subject.mesh | Surface Properties | en_HK |
dc.subject.mesh | Temperature | en_HK |
dc.subject.mesh | Thermometers | en_HK |
dc.title | Temperature and dimensional changes in the two-stage processing technique for complete dentures | en_HK |
dc.type | Article | en_HK |
dc.identifier.openurl | http://library.hku.hk:4550/resserv?sid=HKU:IR&issn=0300-5712&volume=23&spage=245&epage=253&date=1995&atitle=Temperature+and+dimensional+changes+in+the+two-stage+processing+technique+for+complete+dentures | en_HK |
dc.identifier.email | Chow, TW:twchow@hku.hk | en_HK |
dc.identifier.authority | Chow, TW=rp00009 | en_HK |
dc.description.nature | link_to_subscribed_fulltext | - |
dc.identifier.doi | 10.1016/0300-5712(95)91190-X | - |
dc.identifier.pmid | 7629330 | en_HK |
dc.identifier.scopus | eid_2-s2.0-0029356096 | en_HK |
dc.identifier.hkuros | 14829 | en_HK |
dc.identifier.volume | 23 | en_HK |
dc.identifier.issue | 4 | en_HK |
dc.identifier.spage | 245 | en_HK |
dc.identifier.epage | 253 | en_HK |
dc.identifier.isi | WOS:A1995RF91200009 | - |
dc.publisher.place | United Kingdom | en_HK |
dc.identifier.scopusauthorid | Yeung, KC=7202424959 | en_HK |
dc.identifier.scopusauthorid | Chow, TW=7203012369 | en_HK |
dc.identifier.scopusauthorid | Clark, RKF=7406318698 | en_HK |
dc.identifier.issnl | 0300-5712 | - |