File Download
There are no files associated with this item.
Links for fulltext
(May Require Subscription)
- Publisher Website: 10.1021/cm970463c
- Scopus: eid_2-s2.0-0001212053
- WOS: WOS:000072634300013
- Find via
Supplementary
- Citations:
- Appears in Collections:
Article: Synthesis and Characterization of New Soluble Polyimides from 3,3′,4,4′-Benzhydrol Tetracarboxylic Dianhydride and Various Diamines
Title | Synthesis and Characterization of New Soluble Polyimides from 3,3′,4,4′-Benzhydrol Tetracarboxylic Dianhydride and Various Diamines |
---|---|
Authors | |
Issue Date | 1998 |
Citation | Chemistry of Materials, 1998, v. 10, n. 3, p. 734-739 How to Cite? |
Abstract | New soluble polyimides were prepared from a series of diamines and a tetracarboxylic dianhydride with a benzhydrol unit, 3,3′,4,4′-benzhydrol tetracarboxylic dianhydride (BHTDA), by one-step method polymerization. The diamines containing flexible units, bulky substituents, and/or noncoplanar conformation unit were prepared by the reaction of the corresponding bisphenol precursors and p-chloronitrobenzene, followed by catalytic reduction of the dinitro compounds. The polyimides obtained were soluble in various solvents such as N-methyl-2-pyrrolidone, N,N-dimethylacetamide, N,N-dimethylformamide, dimethyl sulfoxide, pyridine, γ-butyrolactone, m-cresol, and even tetrahydrofuran except for polymer PId. The polymers were amorphous and had number-average molecular weight (M ) in the range (3.0-10.2) × 10 . The glass transition temperatures (T ) of the polymers ranged from 268 to 341 °C. These polymers exhibited good thermal stability without significant weight loss up to 420 °C. The temperatures at 10% weight loss range from 457 to 524 °C in nitrogen and 449 to 519 °C in air, respectively. The polyimide films were found to be transparent, flexible, and tough. The films had a tensile strength range 72-105 MPa, an elongation range at break of 4-7%, and a Young's modulus range of 2.18-2.85 GPa. n g 4 |
Persistent Identifier | http://hdl.handle.net/10722/298387 |
ISSN | 2023 Impact Factor: 7.2 2023 SCImago Journal Rankings: 2.421 |
ISI Accession Number ID |
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Liaw, Der Jang | - |
dc.contributor.author | Liaw, Been Yang | - |
dc.contributor.author | Li, Lain Jong | - |
dc.contributor.author | Sillion, Bernard | - |
dc.contributor.author | Mercier, Régis | - |
dc.contributor.author | Thiria, Remi | - |
dc.contributor.author | Sekiguchi, Hikaru | - |
dc.date.accessioned | 2021-04-08T03:08:19Z | - |
dc.date.available | 2021-04-08T03:08:19Z | - |
dc.date.issued | 1998 | - |
dc.identifier.citation | Chemistry of Materials, 1998, v. 10, n. 3, p. 734-739 | - |
dc.identifier.issn | 0897-4756 | - |
dc.identifier.uri | http://hdl.handle.net/10722/298387 | - |
dc.description.abstract | New soluble polyimides were prepared from a series of diamines and a tetracarboxylic dianhydride with a benzhydrol unit, 3,3′,4,4′-benzhydrol tetracarboxylic dianhydride (BHTDA), by one-step method polymerization. The diamines containing flexible units, bulky substituents, and/or noncoplanar conformation unit were prepared by the reaction of the corresponding bisphenol precursors and p-chloronitrobenzene, followed by catalytic reduction of the dinitro compounds. The polyimides obtained were soluble in various solvents such as N-methyl-2-pyrrolidone, N,N-dimethylacetamide, N,N-dimethylformamide, dimethyl sulfoxide, pyridine, γ-butyrolactone, m-cresol, and even tetrahydrofuran except for polymer PId. The polymers were amorphous and had number-average molecular weight (M ) in the range (3.0-10.2) × 10 . The glass transition temperatures (T ) of the polymers ranged from 268 to 341 °C. These polymers exhibited good thermal stability without significant weight loss up to 420 °C. The temperatures at 10% weight loss range from 457 to 524 °C in nitrogen and 449 to 519 °C in air, respectively. The polyimide films were found to be transparent, flexible, and tough. The films had a tensile strength range 72-105 MPa, an elongation range at break of 4-7%, and a Young's modulus range of 2.18-2.85 GPa. n g 4 | - |
dc.language | eng | - |
dc.relation.ispartof | Chemistry of Materials | - |
dc.title | Synthesis and Characterization of New Soluble Polyimides from 3,3′,4,4′-Benzhydrol Tetracarboxylic Dianhydride and Various Diamines | - |
dc.type | Article | - |
dc.description.nature | link_to_subscribed_fulltext | - |
dc.identifier.doi | 10.1021/cm970463c | - |
dc.identifier.scopus | eid_2-s2.0-0001212053 | - |
dc.identifier.volume | 10 | - |
dc.identifier.issue | 3 | - |
dc.identifier.spage | 734 | - |
dc.identifier.epage | 739 | - |
dc.identifier.isi | WOS:000072634300013 | - |